soldering stainless
deantre
Posted 2/24/2009 11:30 AM (#362427)
Subject: soldering stainless




Posts: 13


trying to find out what solder and flux to use when rewiring topwates like the le lures, etc. Thanks
muskie-nick
Posted 2/24/2009 6:02 PM (#362491 - in reply to #362427)
Subject: RE: soldering stainless





Posts: 163


Location: lake st clair michigan
try this link http://www.muggyweld.com/silversolder.html

Edited by muskie-nick 2/24/2009 6:07 PM
castmaster
Posted 2/24/2009 10:43 PM (#362577 - in reply to #362427)
Subject: Re: soldering stainless





Posts: 910


Location: Hastings, mn, 55033
I use a 60/40 acid core solder for doing stainless wire. The .062 or .081 diameter stuff seems to work best, the .125 diameter seems to be to thick to melt well with the wire.